[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"doc-seo-662725-105":3,"detail-sidebar-cat-0-en-105":81,"doc-detail-662725-en":130},{"code":4,"msg":5,"data":6},0,"ok",{"site_id":7,"language":8,"slug":9,"title":10,"keywords":11,"description":12,"schema_data":13,"social_meta":74,"head_meta":76,"extra_data":78,"updated_unix":80},105,"en","field-welding-procedures-4th-edition-june-2011","FIELD WELDING PROCEDURES - 4th Edition - June 2011","","Approved Field Welding Procedures for NCDOT bridge construction and maintenance. The manual guides NCDOT construction inspectors and welding contractors on acceptable field welding practices, including qualification requirements for personnel, qualification of welds and procedures, workmanship expectations, weld profiles, and repair and cleaning steps. It also covers preheat and interpass temperature, electrode storage, weld acceptance criteria, stud welding, and detailed equipment requirements, referencing governing standards and WPS documents.",{"@graph":14,"@context":73},[15,34,56],{"@type":16,"itemListElement":17},"BreadcrumbList",[18,23,27,31],{"item":19,"name":20,"@type":21,"position":22},"https://docshare.wps.com","Home","ListItem",1,{"item":24,"name":25,"@type":21,"position":26},"https://docshare.wps.com/document/","Document",2,{"item":28,"name":29,"@type":21,"position":30},"https://docshare.wps.com/document/technology/","Technology",3,{"item":32,"name":10,"@type":21,"position":33},"https://docshare.wps.com/document/field-welding-procedures-4th-edition-june-2011/662725/",4,{"url":32,"name":10,"@type":35,"image":36,"author":41,"headline":10,"publisher":44,"fileFormat":47,"inLanguage":8,"description":12,"dateModified":48,"datePublished":49,"encodingFormat":47,"isAccessibleForFree":50,"interactionStatistic":51},"DigitalDocument",{"url":37,"@type":38,"width":39,"height":40},"https://docshare.wps.com/thumbnails/field-welding-procedures-4th-edition-june-2011/662725.png","ImageObject",300,407,{"name":42,"@type":43},"MrHarris58","Person",{"url":19,"name":45,"@type":46},"DocShare","Organization","application/pdf","2026-10-30","2026-10-28",true,{"@type":52,"interactionType":53,"userInteractionCount":55},"InteractionCounter",{"@type":54},"ViewAction",5,{"@type":57,"mainEntity":58},"FAQPage",[59,65,69],{"name":60,"@type":61,"acceptedAnswer":62},"Who is the manual intended to guide and for what purpose?","Question",{"text":63,"@type":64},"The manual is intended to assist the NCDOT Construction Inspector and guide the Welding Contractor with acceptable procedures for field welding on NCDOT bridge projects, and to aid bridge maintenance personnel with repair of existing structures.","Answer",{"name":66,"@type":61,"acceptedAnswer":67},"What authorization or approval process is described for welding procedures and WPS documents?",{"text":68,"@type":64},"A Welding Procedure Specification (WPS) may be generated by an authorized person (e.g., CWI) and submitted to the NCDOT Materials & Tests Unit (Steel Section) at the listed address for approval if the contractor does not want to use the provided material.",{"name":70,"@type":61,"acceptedAnswer":71},"When is field welding required or permitted according to the reference standards?",{"text":72,"@type":64},"Field welding should be performed only when called for on the plans and in accordance with the cited specification section, and welds are expected to be placed where shown or called for unless written approval is received for additional welding.","https://schema.org",{"og:url":32,"og:type":75,"og:title":10,"og:site_name":45,"og:description":12},"article",{"robots":77,"canonical":32},"index,follow",{"doc_id":79,"site_id":7},662725,1793222125,{"code":4,"msg":82,"data":83},"success",[84,88,92,96,100,104,109,114,119,122,126],{"id":22,"doc_module":4,"doc_module_name":25,"category_name":85,"show_sort_weight":86,"slug":87},"Story & Novel",90,"story-novel",{"id":26,"doc_module":4,"doc_module_name":25,"category_name":89,"show_sort_weight":90,"slug":91},"Literature",80,"literature",{"id":33,"doc_module":4,"doc_module_name":25,"category_name":93,"show_sort_weight":94,"slug":95},"Exam",70,"exam",{"id":55,"doc_module":4,"doc_module_name":25,"category_name":97,"show_sort_weight":98,"slug":99},"Comic",60,"comic",{"id":101,"doc_module":4,"doc_module_name":25,"category_name":29,"show_sort_weight":102,"slug":103},6,50,"technology",{"id":105,"doc_module":4,"doc_module_name":25,"category_name":106,"show_sort_weight":107,"slug":108},7,"Healthcare",40,"healthcare",{"id":110,"doc_module":4,"doc_module_name":25,"category_name":111,"show_sort_weight":112,"slug":113},8,"Research & Report",30,"research-report",{"id":115,"doc_module":4,"doc_module_name":25,"category_name":116,"show_sort_weight":117,"slug":118},9,"Religion & Spirituality",20,"religion-spirituality",{"id":117,"doc_module":4,"doc_module_name":25,"category_name":120,"show_sort_weight":117,"slug":121},"World Cup","world-cup",{"id":123,"doc_module":4,"doc_module_name":25,"category_name":124,"show_sort_weight":123,"slug":125},10,"Lifestyle","lifestyle",{"id":127,"doc_module":4,"doc_module_name":25,"category_name":128,"show_sort_weight":55,"slug":129},19,"General","general",{"code":4,"msg":82,"data":131},{"doc_id":79,"user_id":132,"nickname":42,"user_avatar":133,"doc_module":4,"category_id":101,"category_name":29,"doc_title":10,"doc_description":12,"doc_content":134,"file_id":135,"file_url":136,"file_type":137,"file_size":138,"view_count":55,"is_deleted":4,"is_public":22,"is_downloadable":22,"audit_status":22,"page_count":139,"language":140,"language_code":8,"site_id":7,"html_lang":8,"table_of_contents":141,"faqs":142,"seo_title":143,"seo_description":12,"update_tm":80,"read_time":144},687212988360,"https://ap-avatar.wpscdn.com/davatar_276721f389ce27ea32af1340a28f341c","(Steel Section)  \nFIELD WELDING PROCEDURES  \nSunset Beach, NC  \nCleveland, NC  \n(Steel Section)  \nFIELD  \nWELDING  \nPROCEDURES  \n4th Edition-June 2011  \nTable of Contents  \nDescription Page Number  \n\n| Cover Sheet  \u003Cbr>Table of Contents   | T-1   |\n| --- | --- |\n| Introduction   | I-1   |\n| General InformationReference Standards   | G-1   |\n| Qualification of Personnel   | G-1   |\n| Qualification of Welds and Procedures   | G-2   |\n| Workmanship   | G-2, G-3   |\n| Weld Profiles   | G-3   |\n| Repairing Welds   | G-4   |\n| Weld Cleaning   | G-4   |\n| Backing Bar   | G-4   |\n| Preheat and Interpass Temperature   | G-5   |\n| Electrode Storage   | G-5   |\n| Weld Acceptance Criteria   | G-6   |\n| Stud Welding   | G-7   |\n| Equipment Requirements   | G-7   |\n| Welding Procedures  \u003Cbr>H-Pile Welding Procedure (WPS 1)   | 1-1 thru 1-4   |\n| Steel Girder Bearing Plate Welding Procedure (WPS 2)   | 2-1 thru 2-3   |\n| Pipe Pile Welding Procedure (WPS 3)   | 3-1 thru 3-4   |\n| Concrete Girder Sole Plate Welding Procedure (WPS 4)   | 4-1 thru 4-3   |\n| Steel Girder SIP Angle Welding Procedure (WPS 5)   | 5-1 thru 5-3   |\n| Concrete Girder SIP Angle Welding Procedure (WPS 6)   | 6-1 thru 6-3   |\n| Stud Welding Procedure (WPS 7)   | 7-1 thru 7-3   |\n| Fillet Weld Certification Welding Procedure (WPS 8)   | 8-1 thru 8-3   |\n| 3G-4G Plate Certification Welding Procedure (WPS 9)   | 9-1 thru 9-3   |\n| 6G Pipe Certification Welding Procedure (WPS 10)   | 10-1 thru 10-3   |\n| SIP Certification Welding Procedure (WPS 11)   | 11-1 thru 11-3   |\n| Encasement Pipe Welding Procedure (WPS 12)   | 12-1 thru 12-3   |\n| Steel Girder Bearing Plate Weathering Steel (unpainted) Welding Procedure (WPS 13)   | 13-1 thru 13-3   |\n| Overhang Bracket Welding Procedure (WPS 14)   | 14-1 thru 14-3   |\n| Steel Girder SIP Strap Welding Procedure (WPS 15)   | 15-1 thru 15-3   |\n| Pipe Pile Bottom Driving Plate (WPS 16)   | 16-1 thru 16-3   |\n| Pot Bearing Welding Procedure (WPS 17)   | 17-1 thru 17-3   |\n| Soldier Pile Welding Procedure (WPS 18)   | 18-1 thru 18-6   |\n| Single V-Groove with Backing (WPS 21)   | 21-1 thru 21-3   |\n| Single V-Groove with Back Gouge (WPS 22)   | 22-1 thru 22-3   |\n| Double Bevel Groove with Back Gouge (WPS 23)   | 23-1 thru 23-3   |\n| Double V-Groove with Back Gouge (WPS 25)   | 25-1 thru 25-3   |\n| Fillet Weld (WPS 27)   | 27-1 thru 27-5   |\n| Armor Angle Field Splice (WPS 28)   | 28-1 thru 28-3   |\n| Single U-Groove with Back Gouge (WPS 29)   | 29-1 thru 29-3   |\n| Appendix A (Welding Terms and Definitions)   | A-1 thru A-9   |\n| Appendix B (SSPC Standards)  \u003Cbr>Appendix C (Welding Symbols)  \u003Cbr>Appendix D (references, credits and Steel Section contact information)   | D-1   |\n| Appendix E (list of revisions)   | E-1, E-2   |\n\n# Introduction\n\nThe information contained within this book of Approved Welding Procedures is intended toassist the NCDOT Construction Inspector and guide the Welding Contractor with acceptableprocedures and practices for the application of weld in a field environment on NCDOT bridgeprojects. Additional information and procedures have been included to assist BridgeMaintenance Personnel with \"Repair of Existing Structures\". The information is in no wayconsidered to be complete or all encompassing but instead offers aid to some of the mostcommon applications to field welding that are found on NCDOT bridge construction projects. AWelding Procedure Specification (WPS) may be generated by an authorized person (i. e. CWI)and then submitted to the NCDOT Materials & Tests Unit (Steel Section) at 770A Park CentreDrive in Kernersville, NC 27284 (phone: 336-993-2300) for approval in the event that thecontractor does not want to utilize the material provided.  \nThese approved welding procedures may also be found at the following web address:  \nhttp://www.ncdot.org/doh/operations/materials/structural/appr_proc.html  \nThis manual may also be found at the following web address:  \nhttp://www.ncdot.org/doh/operations/materials/pdf/","cbCaiaMLaL2OTvvi","https://ap.wps.com/l/cbCaiaMLaL2OTvvi","pdf",9798516,156,"English","# Introduction\n# General Information\n## Reference Standards\n# Qualification of Personnel\n## Personnel testing and approval\n# Qualification of Welds and Procedures\n# Workmanship\n# Weld Profiles\n# Repairing Welds\n# Weld Cleaning\n# Backing Bar\n# Preheat and Interpass Temperature\n# Electrode Storage\n# Weld Acceptance Criteria\n# Stud Welding\n# Equipment Requirements\n# Welding Procedures","[{\"question\":\"Who is the manual intended to guide and for what purpose?\",\"answer\":\"The manual is intended to assist the NCDOT Construction Inspector and guide the Welding Contractor with acceptable procedures for field welding on NCDOT bridge projects, and to aid bridge maintenance personnel with repair of existing structures.\"},{\"question\":\"What authorization or approval process is described for welding procedures and WPS documents?\",\"answer\":\"A Welding Procedure Specification (WPS) may be generated by an authorized person (e.g., CWI) and submitted to the NCDOT Materials \\u0026 Tests Unit (Steel Section) at the listed address for approval if the contractor does not want to use the provided material.\"},{\"question\":\"When is field welding required or permitted according to the reference standards?\",\"answer\":\"Field welding should be performed only when called for on the plans and in accordance with the cited specification section, and welds are expected to be placed where shown or called for unless written approval is received for additional welding.\"}]","FIELD WELDING PROCEDURES - 4th Edition - June 2011 | PDF",393]